Lead and Zinc ore dressing – ZJH minerals
A. Grinding argillaceous zinc oxide ore to make the particle size of -0.1mm account for 50% ~ 80%; B. Flotation of lead oxide by classifying and overflowing the pulp; C. Put the lead flotation tailings into the agitation tank, control the pulp concentration at 25 ~ 35%, add flotation agent, control the pH value of the pulp 9-11, and stir for 6 ...